Galvanostatic EIS (GEIS)

Electrochemical Impedance Spectroscopy (EIS) is an electrochemical technique that measures the impedance of a system as a function of AC current frequency. EIS enables the separation of different component influences, including contributions from electron transfer resistance, double layer capacitance, and other electrochemical processes.

GEIS applies a galvanostatic sinusoidal excitation signal and analyzes the resulting potential response from the device under test (DUT). The density parameter determines the number of measurement points within a specified frequency range. Averaging multiple sine waves reduces noise and non-systematic interference, although this increases the total measurement time.

Galvanostatic EIS is ideal for devices under test (DUT) with low impedances, such as fuel cells, electrolysis cells, batteries, and supercapacitors. High capacitance devices exhibit very long relaxation times. A drifting open circuit voltage (OCV) can cause very high equalizing currents in low impedance devices.

Parameter Description

Parameter

Name

Description

Unit

I dc bias

DC bias current

DC bias current for defining the operating point of the object
set to zero for state of charge

A

I amplitude

amplitude

AC current peak amplitude
sine wave stimulation is from bias-amplitude to bias+amplitude

A

f start

start frequency

starting frequency of the impedance spectrum
useful to check system stability by forward and backward scan

Hz

f max

maximum frequency

upper frequency limit of the impedance spectrum

Hz

f min

minimum frequency

lower frequency limit of the impedance spectrum
most effect on EIS runtime

Hz

t meas

minimum measurement time

minimum recording time for each frequency step
allow more averages at higher frequencies

s

N waves

minimum averages

minimum number of sine waves for each frequency step
more averages for higher SNR

Density >66Hz

density above 66 Hz

number of frequency steps per decade between 66 Hz and f max
frequency steps are logarithmic equidistant

Density at f min

density at f min

number of frequency steps per decade at f min
logarithmic linear density from f min to 66 Hz

A Start Phase Galvanostatic can be enabled or disabled before the method is executed.

Diagram of the galvanostatic EIS measurement, illustrating the galvanostatic sinusoidal excitation signal applied to the device under test across the swept frequency range.

Measurement Result

The measurement results can be displayed as either Nyquist or Bode plots. To evaluate the spectra, the measurement data is fitted to a representative equivalent circuit model of the DUT. This approach enables the determination of detailed individual parameters for each equivalent circuit element.