Current-Voltage Curves
This example demonstrates how to measure current-voltage curves using the zahner_link library with your IM7 potentiostat.
These measurements are known by various names depending on the specific technique used. In the zahner_link API, all these techniques are implemented as ramps with different parameters as the RampJob. Common names include:
Current-Voltage Curves (I-V/IE)
Galvanostatic Ramp
Potentiostatic Ramp
Linear Sweep Voltammetry (LSV)
Linear Sweep Galvanostatic
Staircase Voltammetry
Staircase Galvanostatic
For stairs with stability criteria per step, there is the SteadyStairsJob, which can be used to map the following methods, among others:
Steady State Staircase Voltammetry
Steady State Staircase Galvanostatic
In this notebook, you’ll learn how to:
Connect to an IM7 electrochemical workstation
Run a galvanostatic linear ramp using RampJob
Run a Steady State Staircase Voltammetry SteadyStairsJob with current stop criteria
Perform a potentiostatic staircase ramp (Cyclic Voltammetry) using CvJob with current limits
Process staircase data to extract endpoint values for clearer analysis
Create different plots of your data (time-based, voltage vs. current, and logarithmic plots)
For file saving and other basic operations, please see our other example notebooks.
Let’s start by defining two helper functions that will make plotting our measurement data easier.
import sys
import matplotlib.pyplot as plt
from matplotlib.ticker import EngFormatter
from typing import Optional, List
import numpy as np
import zahner_link as zl
def plot_dataset_tiu(dataset: zl.DcDataset):
"""Plot voltage and current vs time from a dataset.
This function creates a dual-axis plot showing voltage and current
measurements over time from a DC dataset.
"""
time = dataset.get_dc_track("time")
voltage = dataset.get_dc_track("voltage")
current = dataset.get_dc_track("current")
fig, ax1 = plt.subplots()
ax2 = ax1.twinx()
(line1,) = ax1.plot(time, voltage, color="blue", label="Voltage", marker="x")
(line2,) = ax2.plot(time, current, color="red", label="Current", marker="x")
ax1.legend(handles=[line1, line2])
ax1.xaxis.set_major_formatter(EngFormatter(unit="$s$"))
ax1.yaxis.set_major_formatter(EngFormatter(unit="$V$"))
ax1.set_xlabel("Time")
ax1.set_ylabel("Voltage")
ax2.xaxis.set_major_formatter(EngFormatter(unit="$s$"))
ax2.yaxis.set_major_formatter(EngFormatter(unit="$A$"))
ax2.set_xlabel("Time")
ax2.set_ylabel("Current")
fig.set_size_inches(18, 10)
plt.show()
return
def plot_dataset_ui(dataset: zl.DcDataset):
"""Plot current vs voltage from a dataset.
This function creates a standard current-voltage plot (I-V curve)
from a DC dataset.
"""
time = dataset.get_dc_track("time")
voltage = dataset.get_dc_track("voltage")
current = dataset.get_dc_track("current")
fig, ax1 = plt.subplots()
(line1,) = ax1.plot(voltage, current, color="blue", marker="x")
ax1.xaxis.set_major_formatter(EngFormatter(unit="$V$"))
ax1.yaxis.set_major_formatter(EngFormatter(unit="$A$"))
ax1.set_xlabel("Voltage")
ax1.set_ylabel("Current")
fig.set_size_inches(18, 10)
plt.show()
return
Connecting to the IM7 and Setting Up
Now we’ll connect to the IM7 potentiostat and set it up for our first measurement. We’ll start in galvanostatic mode (current control) for our first current-voltage curve.
link = zl.ZahnerLinkExc("10.10.253.150", "1994")
try:
link.connect()
print("connected successfully")
except zl.ZahnerLinkException as e:
error_object: zl.ErrorObject = e.error
print(f"failed to connect, status: {error_object.get_error_code_enum()}, message: {error_object.get_message_formatted()}")
sys.exit()
switch_on_job = zl.control.SwitchOnJob(
potentiostat="MAIN:1:POT",
coupling=zl.PotentiostatCoupling.GALVANOSTATIC,
bias=0,
voltage_range_index=0,
compliance_range_index=0,
)
switch_off_job = zl.control.SwitchOffJob(potentiostat="MAIN:1:POT")
link.do_job(switch_on_job)
connected successfully
<zahner_link._zahner_link.ErrorObject at 0x25b3d4fed30>
Galvanostatic Linear Sweep
With the potentiostat in galvanostatic mode, we’ll run a linear current ramp from 0 A to 1 A using the RampJob.
We’re configuring the ramp with these parameters:
start_valueandend_value: Define our ramp range (0 A to 1 A)scan_rate: How fast to sweep (0.1 A/s)step_height: Set to 0, instructing the IM7 to use the smallest possible step size with its 32-bit DACoutput_data_rate: How many data points per second to record (10 Hz)
After the measurement completes, we’ll plot the results in two ways: time vs. voltage/current and voltage vs. current.
linear_ramp_job = zl.meas.RampJob(
start_value=0, # Start at 0 A
end_value=1, # End at 1 A
scan_rate=0.1, # 0.1 A per second
step_height=0, # Let IM7 choose smallest step size
output_data_rate=10, # 10 points per second
autorange=True, # Auto-select measurement ranges
current_range=0.1, # Only used if autorange=False
)
link.do_job(linear_ramp_job)
linear_ramp_data = link.get_job_result_data(linear_ramp_job)
plot_dataset_tiu(linear_ramp_data)
plot_dataset_ui(linear_ramp_data)
Steady State Staircase
Instead of a linear sweep with constant scanning, it is also possible to take measurements at discrete values and apply a stability criterion before proceeding to the next value. For this job, we will also switch to potentiostatic mode (voltage control).
This allows measurements to be taken at different voltages until the current stabilizes. This is accomplished using the SteadyStairsJob.
The staircase with stability criteria is combined with a MinMaxLimitStopCondition to stop the staircase if the absolute maximum current of 1 A is exceeded.
Stop conditions allow measurements to be terminated early, before their configured runtime, based on various criteria. For example, a constant current polarization can be stopped once a specific voltage limit is reached. Another example is an OCV scan that automatically stops when the open-circuit voltage has stabilized.
Various stop conditions are available; the most important ones are:
MinMaxLimitStopCondition - stops the measurement when a minimum or maximum value is reached.
StabilityToleranceLimitStopCondition - stops the measurement when a value has stabilized.
link.do_job(switch_off_job)
switch_on_job.parameters.coupling = zl.PotentiostatCoupling.POTENTIOSTATIC
link.do_job(switch_on_job)
stop_conditions = [
zl.meas.stop.MinMaxLimitStopCondition(
for_dimension="current", minimum=-1, maximum=1
) # stop at a absolute maximum current of 1 A
]
steady_stairs_job = zl.meas.SteadyStairsJob(
start_value=0, # Start at 0 V
end_value=1, # End at 1 V
step_time=2, # maximum of 2 seconds
step_height=0.01, # 10 mV steps
hold_time=1, # at least 1 second
stability_tolerance=0.01, # 10 mA/s stability criterion
output_data_rate=10, # 10 points per second
autorange=False, # no autorange, use fixed ranges
current_range=1, # fixed current range of 1 A
stop_conditions=stop_conditions,
)
try:
link.do_job(steady_stairs_job)
except zl.ZahnerLinkException as e:
error_object: zl.ErrorObject = e.error
if error_object.get_error_code_enum() == zl.ErrorCodeEnum.STOP_CONDITION_TRIGGERED:
print(f"successfully stopped on stop condition, error code: {error_object.get_error_code_enum()}, message: {error_object.get_message_formatted()}")
steady_stairs_data = link.get_job_result_data(steady_stairs_job)
plot_dataset_tiu(steady_stairs_data)
plot_dataset_ui(steady_stairs_data)
In the previous plot, which shows current and voltage as a function of time, the longer steps are clearly visible at higher currents.
It’s also apparent that the staircase measurement is immediately terminated after a current greater than 1 A is measured.
The following code retrieves information about why the job was stopped, in this case due to the stop condition:
info = steady_stairs_job.get_last_job_info()
error = info.get_error()
if error and error.get_error_code_enum() == zl.ErrorCodeEnum.STOP_CONDITION_TRIGGERED:
print(f"Error code: {error.get_error_code_enum()}")
print(error.get_message_formatted())
print(error.get_message_format_string())
print(error.get_message_parameters())
triggered_stop_condition = stop_conditions[error.get_message_parameters()[0]]
print(f"Triggered stop condition: {triggered_stop_condition}")
Error code: ErrorCodeEnum.STOP_CONDITION_TRIGGERED
stop condition #0 triggered: current: 1.16889 < -1 or 1.16889 > 1
stop condition #{0} triggered: {1}
[0, 'current: 1.16889 < -1 or 1.16889 > 1']
Triggered stop condition: <zahner_link._zahner_link.meas.stop.MinMaxLimitStopCondition object at 0x0000025B3D4FFC70>
Potentiostatic Ramps
Now we’ll use the CvJob to perform multiple ramps. Note that the RampJob could also be used.
Important Note: The behavior of CvJob adapts to the potentiostat’s operating mode:
In potentiostatic mode: Parameters like
start_valuecontrol voltage, and boundary parameters control currentIn galvanostatic mode: Parameters like
start_valuecontrol current, and boundary parameters control voltage
For our staircase voltammetry, we’ll use:
step_height: 0.01 V to create discrete voltage stepsturn_limit_check: Enabled to protect our sample by setting current limitsupper_turn_boundaryandlower_turn_boundary: +1 A and -1 A limits
This will perform a triangular voltage sweep from 0V → +0.5V → -0.5V → 0V, but will reverse direction earlier if current exceeds either limit.
stairs_height = 0.01
stairs_ramp_job = zl.meas.CvJob(
start_value=0,
first_vertex=0.5,
second_vertex=-0.5,
end_value=0,
scan_rate=0.01,
output_data_rate=10,
num_cycles=0.5,
autorange=True,
current_range=1,
turn_limit_check=True,
upper_turn_boundary=1,
lower_turn_boundary=-1,
step_height=stairs_height,
ir_drop=0,
)
link.do_job(stairs_ramp_job)
stairs_ramp_data = link.get_job_result_data(stairs_ramp_job)
plot_dataset_tiu(stairs_ramp_data)
plot_dataset_ui(stairs_ramp_data)
Switch Off and Disconnect
Now that we’ve completed our measurements, let’s properly shut down by turning off the potentiostat and disconnecting from the IM7.
Note that disconnecting doesn’t affect our measurement data - we can still access it from the job objects we created earlier.
link.do_job(switch_off_job)
link.disconnect()
Advanced Data Processing for Staircase Measurements
Staircase ramps produce data with transient current spikes whenever the voltage changes. These transients can make it difficult to see the true steady-state relationship between voltage and current.
To get cleaner results, we’ll extract only the current values measured at the end of each voltage step, when the transients have settled. This gives us a better representation of the steady-state response.
We’ll define two helper functions:
find_step_endpoints: Identifies the last data point in each voltage step before the voltage changesget_step_values: Extracts these specific endpoint values from our raw data arrays
stair_voltage = stairs_ramp_data.get_dc_track("voltage")
stair_current = stairs_ramp_data.get_dc_track("current")
def find_step_endpoints(
data: List[float],
step_height: float,
min_value: Optional[float] = None,
max_value: Optional[float] = None,
) -> np.array:
"""
Find the indices where each step ends in a staircase signal.
This function analyzes a staircase signal and identifies the last
data point of each step before the signal changes to the next level.
:param data: The signal to analyze (e.g., voltage measurements)
:param step_height: The height of each step (e.g., 0.01V)
:param min_value: Optional minimum value (auto-detected if None)
:param max_value: Optional maximum value (auto-detected if None)
:return: Array of indices marking the end of each step
"""
signal = np.array(data)
if min_value is None:
min_value = np.min(signal)
if max_value is None:
max_value = np.max(signal)
lowest_bin = np.floor(min_value / step_height) * step_height
highest_bin = np.ceil(max_value / step_height) * step_height
bin_centers = np.arange(lowest_bin, highest_bin + step_height, step_height)
bin_edges = np.concatenate(
[bin_centers - step_height / 4, [bin_centers[-1] + step_height / 4]]
)
bin_edges.sort()
bin_indices = np.digitize(signal, bin_edges)
endpoints = []
current_bin = bin_indices[0]
for i in range(1, len(signal)):
if bin_indices[i] != current_bin:
endpoints.append(i - 1)
current_bin = bin_indices[i]
elif i < len(signal) - 1:
next_bin = bin_indices[i + 1]
if next_bin != current_bin:
endpoints.append(i)
if not endpoints or endpoints[-1] != len(signal) - 1:
endpoints.append(len(signal) - 1)
return np.array(endpoints)
def get_step_values(data: List[float], indexes: List[int]) -> np.array:
"""
Extract values at specific indices from a data array.
:param data: The source data array
:param indexes: The indices to extract
:return: Array containing only the values at the specified indices
"""
return np.array([data[i] for i in indexes])
Now let’s use these functions to process our staircase measurement data. We’ll find the endpoint of each voltage step and extract the corresponding voltage and current values.
endpoints_on_steps = find_step_endpoints(stair_voltage, stairs_height)
stair_voltage_end_values = get_step_values(stair_voltage, endpoints_on_steps)
stair_current_end_values = get_step_values(stair_current, endpoints_on_steps)
Creating a Logarithmic Current-Voltage Plot
Finally, let’s visualize our processed data using a logarithmic plot of current vs. voltage. The logarithmic scale for current helps reveal both small and large current values in the same plot, which is especially useful for semiconductor devices and electrochemical systems where current can vary by many orders of magnitude.
fig, ax1 = plt.subplots()
(line1,) = ax1.semilogy(
stair_voltage_end_values,
np.abs(stair_current_end_values),
color="blue",
marker="o",
markersize=3,
linestyle="None",
)
ax1.xaxis.set_major_formatter(EngFormatter(unit="$V$"))
ax1.yaxis.set_major_formatter(EngFormatter(unit="$A$"))
ax1.set_xlabel("Voltage")
ax1.set_ylabel("|Current|")
ax1.grid()
fig.set_size_inches(18, 10)
plt.show()